Technical Demonstration: Experiments and Analysis on the Hysitron TI 980 TriboIndenter
- [00:00:00] Indentation Curve to Stress and Strain Relationship
- [00:01:41] Spherical Indentation Stress-Strain
- [00:11:44] The Onset of Plasticity: High-Load Indentation and In-Situ SPM Imaging
- [00:24:21] Experimental Considerations for Accurate Stress-Strain Analysis
 
 
Stress-Strain Curves Derived from Indentation Force-Displacement Data
 Presented by Dr. André Clausner
- [00:26:06] Introduction
- [00:27:54] Representative Strain and Stress
- [00:33:07] Constraint Factor 
- [00:42:01] Inverse Finite Element Modelling
- [00:48:42] Machine Learning-Based Methods
- [00:54:18] Summary