Bruker
▶ Watch On-Demand | 50 Minutes

In-Situ Nanoindentation Virtual Workshop: Advanced Capabilities of the New Hysitron PI 89 PicoIndenter

Discover the advanced in-situ nanoindentation capabilities of the Hysitron PI 89 PicoIndenter.
Presented by Ude Hangen, Ph.D., Applications Manager, Bruker; Jaroslav Lukes, Ph.D., Applications Scientist, Bruker; and Rhys Jones, Ph.D., Product Specialist, Bruker (December 01, 2021)

       PRESENTATION HIGHLIGHTS:

  • [00:00:00] Intro & virtual showroom spotlight 
  • [00:02:39] In depth look at the Hysitron PI 89 PicoIndenter
  • [00:15:04] Demonstration introduction
  • [00:16:41] Hysitron PI 89 demonstration setup
  • [00:19:15] Pillar compression test
  • [00:27:19] Analyzing pillar compression tests
  • [00:30:55] Generating a hardness map using automated indentation
  • [00:45:13] Analyzing automated indentation tests
  • [00:46:48] Closing

Related Resources

Application Notes