In-Situ Nanoindentation Virtual Workshop: Advanced Capabilities of the New Hysitron PI 89 PicoIndenter
Discover the advanced in-situ nanoindentation capabilities of the Hysitron PI 89 PicoIndenter.
このビデオを再生するには Cookie を受け入れる必要があります
Presented by Ude Hangen, Ph.D., Applications Manager, Bruker; Jaroslav Lukes, Ph.D., Applications Scientist, Bruker; and Rhys Jones, Ph.D., Product Specialist, Bruker (December 01, 2021)
PRESENTATION HIGHLIGHTS:
[00:00:00] Intro & virtual showroom spotlight
[00:02:39] In depth look at the Hysitron PI 89 PicoIndenter
[00:15:04] Demonstration introduction
[00:16:41] Hysitron PI 89 demonstration setup
[00:19:15] Pillar compression test
[00:27:19] Analyzing pillar compression tests
[00:30:55] Generating a hardness map using automated indentation