Nanomechanical Testing Webinars

Dynamic Mechanical Characterization of Polymer Coatings and Thin Films via Nanoindentation

Join Yusuke Matsuda (DuPont Electronics and Industrial) for a review of NanoDMA III for industrial applications with comparisons to macroscale DMA


The time dependence in polymers is different from that of metals or ceramics. As a result, testing their mechanical properties requires a different approach than traditional indentation.

This webinar focuses on the verification of nanoscale dynamic mechanical analysis (nanoDMA III) for industrial polymer thin films using both time and temperature variation and in comparison to macroscale tensile DMA.

Input value is invalid.

The full-length recording of this presentation is available for on-demand viewing.

 

Please enter your first name
Please enter your last name
Please enter your e-mail address
Please enter a valid phone number
Please enter your Company/Institution
What best describes your current interest?
Please add me to your email list for webinar invitations, product announcements, and local event updates.
Please accept the Terms and Conditions

             Privacy Notice   Terms of Use


Note: Page will refresh upon submission; afterward, you may need to scroll down to see the video access link.

* Please fill out the mandatory fields.

NanoDMA III for Polymeric Thin Films in Industrial Applications

The time dependence in polymers requires a different approach to that of traditional indentation of metals. The viscoelasticity, pressure dependence, and contact stiffness are all vastly different than that found in metals or ceramics, and must be taken into account.

In this webinar:

  • The nanoDMA III technique is reviewed, various tip geometries are compared, and experiments are performed using the TI 980 TriboIndenter, with xSol stage;
  • Yusuke Matsuda of DuPont Electronics and Industrial presents on his work verifying nanoscale dynamic mechanical analysis using both time and temperature variation;
  • Multiple approaches to doing small scale mechanics appropriate to polymers and polymetric thin films are reviewed, with comparisons made to macroscale tensile DMA; and
  • Results on industrially relevant materials systems that cannot be tested at the macroscale are presented.

LEARN MORE

Find out more about the technology featured in this webinar or our other solutions for characterizing the nanomechanical properties of materials:

Speaker

Yusuke Matsuda, Ph.D.
DuPont Electronics and Industrial