This webinar recording discusses testing and analysis methods for SRJ tests using the Bruker Hysitron TI 980 TriboIndenter. Functions for necessary data correction were validated using single-crystalline BCC tungsten, but extension to other material systems are also discussed.
Thermally activated deformation processes control plasticity and fracture in many materials, including body-centered cubic (BCC) metals, and can be probed via the strain rate dependence of their yield stress. One technique to probe this is the strain rate jump test, in which the strength change at an abrupt change in applied strain rate is measured, which has traditionally been performed on the bulk scale, but requires large samples and cannot measure local properties. Nanoindentation solves both of those issues.
This webinar will discuss testing methods for strain rate jump tests using the Bruker Hysitron TI 980, as well as functions to perform necessary corrections to the data. The functions were validated using single crystalline BCC tungsten as a model material, so application to other material systems will be discussed.
Find out more about the technology featured in this webinar or our other solutions for Nanomechanical Testing:
Kevin Schmalbach, Ph.D., Staff Scientist, Nanoindentation Unit, Bruker
Kevin earned his PhD in Chemical Engineering from the University of Minnesota in 2022, where his thesis focused on the effects of temperature and strain rate in tungsten. He joined Bruker as a postdoctoral scientist in the Applications Group before transitioning to the Research and Development team as an instrumentation scientist. In this role, he played a key role in developing the PI 89 Auto capabilities as well as supporting hardware innovation and technique development for nanoindentation. He has recently advanced to a staff scientist position within the Applications Group.
David Vodnick
NI Product Line Manager, Bruker