Nanomechanical Testing Webinars

Algorithms for Nanoindentation Strain Rate Jump Testing Using the Hysitron TI 980

Learn more about best practices for localized strain rate jump testing at the nanoscale

Learn how to perform and analyze strain rate jump tests to understand thermally activated deformation processes

This webinar recording discusses testing and analysis methods for SRJ tests using the Bruker Hysitron TI 980 TriboIndenter. Functions for necessary data correction were validated using single-crystalline BCC tungsten, but extension to other material systems are also discussed.

 

Input value is invalid.

The full-length recording of this presentation is available for on-demand viewing.

 

Please enter your first name
Please enter your last name
Please enter your e-mail address
Please enter a valid phone number
Please enter your Company/Institution
What best describes your current interest?
Please add me to your email list for webinar invitations, product announcements, and local event updates.
Please accept the Terms and Conditions

             Privacy Notice   Terms of Use


Note: Page will refresh upon submission; afterward, you may need to scroll down to see the video access link.

* Please fill out the mandatory fields.

Webinar Recording is Now Available.


Note:
If you close or exit this page, you will not be able to reopen this confirmation window without re-submitting the form. Please save this access link to bypass the form in future visits.

Investigate Strain Rate Jump Testing Methods

Thermally activated deformation processes control plasticity and fracture in many materials, including body-centered cubic (BCC) metals, and can be probed via the strain rate dependence of their yield stress. One technique to probe this is the strain rate jump test, in which the strength change at an abrupt change in applied strain rate is measured, which has traditionally been performed on the bulk scale, but requires large samples and cannot measure local properties. Nanoindentation solves both of those issues.

This webinar will discuss testing methods for strain rate jump tests using the Bruker Hysitron TI 980, as well as functions to perform necessary corrections to the data. The functions were validated using single crystalline BCC tungsten as a model material, so application to other material systems will be discussed.

Find out more about the technology featured in this webinar or our other solutions for Nanomechanical Testing:

Speakers
 

Kevin Schmalbach, Ph.D., Instrumentation Scientist, Nanoindentation Unit, Bruker

Kevin earned his PhD in Chemical Engineering from the University of Minnesota in 2022 with his thesis focusing on the study of temperature and strain rate effects in tungsten. He then joined the applications group as a postdoctoral scientist at Bruker, where he developed the PI 89 Auto capabilities. He has recently moved into an instrumentation scientist role in the research and development group, focusing on hardware and technique development for nanoindentation.

David Vodnick